TA2 vs TC4 Titanium: Pure Titanium vs Ti-6Al-4V — Which One Do You Actually Need?

Enquiries arrive worded like this: “Titanium sheet, 4 mm, strongest grade you have.” Or the mirror image: a load-bearing bracket drawing specified in TA2 because somebody’s last supplier had it on the shelf.

Both are the same mistake from opposite ends. TA2 and TC4 share a word, “titanium”, and not much else. One is commercially pure metal chosen for how it survives chemistry. The other is an alloy chosen for how it survives load. Specifying TC4 for a corrosion job buys you strength you will never use and machining bills you will definitely notice. Specifying TA2 for a structural part buys you a part that bends.

What each grade actually is

TA2 is commercially pure titanium under the Chinese GB system, and it corresponds to ASTM Grade 2 — the grade most Western drawings mean when they just say “CP titanium”. It is at least 99.2% titanium; the balance is mostly oxygen (≤0.25%) and iron (≤0.30%), and those interstitials set its strength. Annealed, it gives a tensile strength of at least 345 MPa and yield of at least 275 MPa.

TC4 is Ti-6Al-4V: titanium alloyed with 5.5–6.75% aluminium and 3.5–4.5% vanadium. It corresponds to ASTM Grade 5. In annealed condition to ASTM B348 it delivers at least 895 MPa tensile and 828 MPa yield — roughly two and a half times the strength of TA2. It is the default alloy for aerospace fasteners, airframe parts and medical implants, because nothing else in the family combines that strength with that weight.

One point causes real confusion in cross-border orders: TA2 and Grade 2 are counterparts, as are TC4 and Grade 5, but certificates are written against different standard systems (GB/T versus ASTM). For most commercial work the grades are interchangeable. For work certified to a specific standard, say so on the order, and the material will be tested and certified against it.

Side by side

TA2 (≈ ASTM Grade 2)TC4 / Ti-6Al-4V (≈ ASTM Grade 5)
TypeCommercially pure titaniumAlpha-beta alloy
CompositionTi ≥99.2%, O ≤0.25%, Fe ≤0.30%Al 5.5–6.75%, V 3.5–4.5%, balance Ti
Tensile strength≥345 MPa≥895 MPa (annealed)
Yield strength≥275 MPa≥828 MPa (annealed)
Density4.51 g/cm³4.43 g/cm³
Corrosion resistanceStronger of the two in most chemical service — seawater, wet chlorine, oxidising acidsVery good; a step below CP grades in some reducing/crevice conditions
WeldabilityStraightforward, standard practiceWeldable; shielding and cleanliness need care
FormabilityCold-forms well — dished ends, tube bendingLimited cold forming; severe springback, usually hot-formed
MachinabilityDifficult, like all titaniumHarder again — tool wear and heat
Heat treatmentCannot be strengthened by heat treatmentHeat-treatable; usually supplied annealed
Relative costLower — material and machining bothHigher — material and machining hours both
Typical usesHeat exchanger tubes and plates, chemical vessels, desalination, marine hardware, electroplating jigsAerospace fasteners and structures, medical implants, high-load shafts, springs, motorsport parts

Corrosion jobs and strength jobs

Sort the application first, and the grade usually sorts itself.

If the part’s enemy is the medium flowing through or around it — seawater in a heat exchanger, chlorine in a chemical line, acid in a pickling tank — TA2 is not the budget option. It is the correct engineering choice. Its corrosion resistance in those media is at least as good as TC4’s and in some conditions better, it welds without drama, it cold-forms into the shapes process equipment actually needs, and it costs less per kilo to start with. Adding vanadium and aluminium buys nothing the medium cares about.

If the part’s enemy is load — a fastener that must not yield, a shaft, a spring, a bracket where the designer counted every gram — TA2 simply cannot do the work. No heat treatment will raise its strength; purity sets a ceiling. That is TC4’s home ground, and its strength-to-weight ratio is why aerospace keeps specifying it.

The grey zone is parts that see both: marine hardware under load, subsea fittings, pump components in seawater. Both grades survive the seawater; the deciding factor is whether the section sizes TA2 needs are acceptable. If the design can carry the thicker wall, TA2 wins on cost and weldability. If it cannot, TC4 earns its price.

The processing reality

Welding. TA2 welds the way titanium is supposed to weld: TIG with decent argon coverage, clean material, no special ceremony. TC4 welds too, but it is less forgiving — contamination shows up as brittle weld metal, and the hot zone, including the back of the joint, needs serious shielding.

Forming. TA2 bends, rolls and presses at room temperature, with springback any experienced shop can allow for. TC4’s springback is in another league; tight cold bends crack, and it is routinely hot-formed. If your part is a formed shell rather than a machined block, that difference alone can decide the grade.

Machining. Neither grade machines like steel, and anyone who quotes titanium work on steel cycle times is heading for an argument. Titanium’s low thermal conductivity puts the heat into the tool edge instead of the chip, and both grades gall if speeds and coolant are wrong. TC4 adds higher cutting forces and faster tool wear on top, so the same finished part costs meaningfully more to produce in TC4 — the gap in the invoice is mostly machining time and tooling, not metal. It is the most underestimated line in most titanium budgets.

Decision rules

  • The medium is corrosive and the loads are ordinary: TA2.
  • The part carries serious load, or weight is being designed out: TC4.
  • The part is welded and formed from sheet or tube: TA2, unless the strength calculation forbids it.
  • The part is machined from solid and the strength is not needed: ask why TC4 is on the drawing before paying to machine it.
  • The drawing names a GB grade and your standard is ASTM (or the reverse): confirm the counterpart in writing — TA2 ↔ Grade 2, TC4 ↔ Grade 5 — and certify to the standard your customer will audit.

What we supply

DILI Industrial Supply Chain Co., Ltd. (DILI Steel), in Suzhou, China, supplies titanium in sheet and plate, bar, tube, wire and forgings — mainly TA2 and TC4, plus neighbouring grades for less common drawings. Parts that need machining can be supplied as custom parts made to drawing, and if there is no drawing yet, our engineers can prepare one from a sample or sketch. There is no minimum order quantity, and every order goes through a pre-shipment inspection with the mill certificate checked against the material before it leaves. Weighing TA2 against TC4 on a live enquiry? Send the drawing or service conditions to [email protected] and we will tell you which way we would go, and why.

FAQ

Is TC4 the same as Grade 5?

Yes, for ordering purposes: TC4 is the GB designation for Ti-6Al-4V, Grade 5 the ASTM designation for the same alloy. Composition and annealed strength line up; what differs is the standard the certificate is written to — GB/T versus ASTM (typically B265 or B348). If your customer audits against a named standard, state it on the order.

Which is better for seawater?

TA2. Commercially pure titanium’s record in seawater — heat exchangers, desalination, marine hardware — is exactly why the grade exists, and TC4 offers no corrosion advantage to justify its cost there. Use TC4 in seawater only when the part also carries loads TA2’s sections cannot handle.

Why is TC4 so much more expensive to machine?

Three things stack up: the alloy itself costs more per kilo; its strength raises cutting forces; and like all titanium it conducts heat poorly, so the tool edge takes the temperature and wears fast. On a machined part, that processing gap is usually bigger than the material price gap — which is why over-specifying TC4 on a corrosion part gets expensive so quickly.

Request your free consultation & quotation

ON THIS PAGE

MORE ARTICLES

Small assorted metal pieces being packed for shipment

Every buyer of metal has had the same moment. You need 200 kg of something — a couple of plates,

Nickel alloy bars and a machined ring in a warehouse

The enquiry usually arrives with the alloy already chosen. A pump shaft for seawater service, specified in Inconel 718 “because

Stainless steel sheets stacked in a warehouse near the coast

Most enquiries we see for 316L do not actually need 316L. And a good share of the 304 that gets

Pre-shipment inspection — measuring a stainless steel plate with a caliper next to its mill test certificate

Almost every “wrong material” dispute has the same shape. The goods arrive, the mill certificate gets filed away unread, and

Talk to DILI

Tell us what you need — we'll take it from there.

Confidential — reviewed only by our engineering & legal desk.

Urgent case

Non-conforming stock or a supplier gone dark?

Confidential — reviewed only by our engineering & legal desk.